Fusion power breakthrough successfully repeated

For the second time, U.S. researchers have achieved net energy gain in a nuclear fusion reaction. The amazing feat, which uses lasers to fuse two atoms, brings investigators one step closer to discovering a near-limitless, safe, and clean source of energy.

One Minute Mentor: Distortion in Tool Steels

Distortion in tool steels encompasses all irreversible dimensional changes. There are two main types: size distortion and shape distortion. Size distortion involves expansion or contraction in volume or linear dimensions without changes in geometrical form. Shape distortion entails changes in curvature or angular relations, as in twisting, bending, and/or nonsymmetrical changes in dimensions. In most […]