The transformation behavior of retained austenite in M2 steel was examined under varying tempering conditions. The steel was initially subjected to interrupted quenching at 105 °C (225 °F), a process that elevated the retained austenite content to approximately 55 vol %, compared to the typical 25 vol % observed after direct quenching to room temperature. This was followed by […]

SECO/WARWICK India Wins New Contract as Shital Vacuum Treat Adds Third Vacuum Furnace

SECO/WARWICK India has secured a new order from Shital Vacuum Treat Pvt Ltd, marking the third time the Indian heat-treatment specialist has chosen SECO/WARWICK’s vacuum furnace technology. The newly ordered furnace will support a wide range of processes including vacuum hardening, tempering, solution treatment, aging, annealing, brazing, and high-pressure gas quenching. Designed to meet NADCA […]

Aichelin Group to acquire Nitrex Heat Treating Solutions and UPC-Marathon

Aichelin Group, Mödling, Austria, has signed an agreement to acquire the Nitrex Heat Treating Solutions (NTS) and UPC-Marathon (UPC) divisions of Montreal-based Nitrex. The acquisition aims to strengthen Aichelin’s global footprint in heat treatment systems and expand its technology portfolio with advanced nitriding and process control capabilities. The strategic move brings together two highly complementary […]

Ipsen promotes seven field service engineers to senior roles

Ipsen, Cherry Valley, IL, announced the promotion of seven field service engineers to the role of senior field service engineer, recognizing their technical expertise, leadership, and dedication to customer service. The newly promoted team members include Matt Hopkins, Jesse Lawrence, Larry Dahm, Glenn Hawkins, Mike Dawson, Daniel Greifemberg, and Craig Ludewig. These promotions reflect Ipsen’s […]

Solar Atmospheres adds new 10-bar vacuum furnace at South Carolina facility

Solar Atmospheres, Greenville, SC, announced the installation and commissioning of a new 10-bar vacuum furnace at its Southeast facility. Designed and built by sister company Solar Manufacturing, the advanced horizontal furnace expands the company’s capacity to process large, high-performance materials, particularly titanium and specialty alloys. The furnace features a working zone measuring 48 inches wide […]