Researchers at the U.S. Department of Energy’s Argonne National Laboratory, Lemont, Ill., have developed a method to coat sulfide-based solid electrolytes, finding a thin, glass-like layer could be the key to longer-lasting, cost-effective solid-state batteries.
Lam Research introduces VECTOR TEOS 3D to address critical advanced packaging challenges in chipmaking
The “soft side” of chips: NIST advances polymer science for semiconductor packaging
Exosens expands technology portfolio
The Engineering Laboratories of NASA’s Kennedy Space Center
The NASA Laboratories, Development and Testing Division provides science and engineering services to NASA programs and projects, contractor partners, and external customers such as other government agencies, aerospace companies, and academia.