Metalysis, England, is powering up the world’s first commercial plant based on solid-state production (Cambridge process) of metal alloy powders at its Materials Manufacturing Centre in Wath upon Dearne, South Yorkshire.
Metalysis, England, is powering up the world’s first commercial plant based on solid-state production (Cambridge process) of metal alloy powders at its Materials Manufacturing Centre in Wath upon Dearne, South Yorkshire.