Grand View Research Inc., San Francisco, has published a thermal spray coating market analysis that predicts the market is expected to reach $12.29 billion by the year 2022.
October 2015 Issue of Advanced Materials & Processes, featuring: Failure Analysis of a Fractured Pin, Furnace Roll Failure on Hot-Dip Coating Line Spurs New Design and Welding Process; Metallurgy Lane: Pioneers in Metals Research-Part II