Nikon Instruments Inc., Melville, N.Y., has added two new stereomicroscope systems to its product portfolio.
AK Steel engineer and ASM member Grant Thomas wins award for steel-quenching research paper
AK Steel, West Chester, Ohio, announces that Research Engineer and ASM International member Grant Thomas, Ph.D., has received the AISI “Finalist Medal” for the technical paper titled, “Tensile Properties Obtained by Quench & Partition Processing of Mn-Ni Steels at Room Temperature Quench Temperatures.”
ASM Fellow Dr. Pradeep Rohatgi elected Fellow of Wisconsin Academy of Sciences
Severstal to sell its steel plants in Michigan and Mississippi