Shape-memory polymers exhibit triple shape-memory behavior

Oak Ridge National Laboratory, Tenn., reports that a team of researchers from ORNL, Washington State University, and the University of Idaho, have developed shape-memory polymers that exhibit triple-shape-memory behavior, meaning that the polymers can transform from one temporary shape to another at one temperature, and then back to a permanent shape at a different temperature.