Ipsen, Cherry Valley, Ill., recently shipped a Titan vacuum furnace system with two-bar gas quenching and PdMetrics predictive maintenance software platform to a company on the West Coast, where it will be used to manufacture components and systems for the aerospace industry.
Advanced Heat Treat completes Phase I of plasma nitriding evaluation
Can-Eng installs T7 heat treatment system for HPDC aluminum auto structures
Furnacare opens advanced vacuum furnace hot-zone rebuild and service center
One Minute Mentor: Stabilization of Ferritic Stainless Steels
Stabilization is generally considered to be the simple gettering of carbon and nitrogen by a suitable carbide former such as titanium or niobium. Stabilization is essential for ferritic stainless steels to avoid the precipitation of grain boundary carbides.