Commercial Metals Co., Irving, Texas, announces that it has begun construction of an electric-arc-furnace steel micromill in Durant, Okla., to produce long products by its continuous-continuous manufacturing process in which steel is melted, cast, and rolled from a single uninterrupted strand.
Ipsen Argos low-pressure carburizing plus 20-bar nitrogen quenching increases hardness
Ipsen, Cherry Valley, Ill., announces that its Global Development Team in Kleve, Germany, recently celebrated the first build and testing of the Argos heat treating system, in which low-pressure carburizing combined with 20-bar nitrogen quenching reportedly provides metallurgical properties never before seen in gas quenching systems.