DC Plasma Arc Gun

Direct-current plasma arc guns combine an axially aligned cathode (typically, 1 to 2% thoriated tungsten), an anode/nozzle (typically, oxygen-free high-conductivity copper), and some means to control gas-flow geometry in the arc chamber.