Researchers from the University of Illinois at Urbana-Champaign, the Georgia Institute of Technology, and the University of Tokyo have developed a new “zippered tube” configuration that makes paper structures stiff enough to hold weight yet able to fold flat for easy shipping and storage.
LIFT co-locates at Detroit headquarters
Institute for Advanced Composites Manufacturing Innovation (IACMI) will open a scale-up facility at LIFT.