Computations show that a material made with just the right amounts of hafnium, nitrogen, and carbon would have a melting point of more than 4400 K (7460°F).
NIST hosts first app challenge to improve data access
Researchers looking for information on the properties of methane at high temperatures or the isotopic composition of an element know they can rely on standard reference data from NIST.