Metlab Heat Treating, Niagara Falls, N.Y., announces completion of a successful project with a major crane manufacturer to flame harden the bridge crane wheels for a large overhead multiple bridge crane system. Installed at an aircraft manufacturer, the crane lifts airplanes as they are being assembled. Over 1,500 wheels made of 1045 steel, approximately 6.5 in. O.D. by 2.5 in. wide, were hardened to a hard and uniform outside rim of 425 BHN (HRC 45) and a case depth of 0.125 in. minimum.
Selas Heat Technology relocates manufacturing to Ohio
Fraunhofer test program evaluates coatings for equipment in oil treatment plants
Fraunhofer IWM, Germany, has developed tests of the internal coatings of pipes in various sections of oil treatment plants to determine which materials are best suited to withstand the stresses in each individual section. To assess the corrosion resistance of coatings in a laboratory environment, the researchers apply a number of different tests, such as high heat, strong chemicals, abrasive media, and many others.
Jumping droplets for more efficient power plants
In a completely unexpected finding, Massachusetts Institute of Technology, Cambridge, researchers discovered that tiny water droplets that form on a superhydrophobic surface, and then “jump” away from that surface, carry an electric charge. The finding could lead to more efficient power plants and a new way of drawing power from the atmosphere, they say.
Single-component additive for TSV copper plating reduces cost and prevents defects
Adeka Corp., Japan, has developed a single-component type additive for TSV (Through Silicone Via) copper plating that will bring a reduction in costs, prevent defects, and enable versatility. Semiconductor manufacturers have recently been attempting to achieve a smaller size and higher performance of devices by stacking multiple chips into the 3D structure.