New transistor concept based on metal nanoparticles with energy gaps

Hamburg University, Germany, announces that a group led by Dr. Christian Klinke has succeeded in producing transistors based on metal nanoparticles so small that they no longer show their metallic character under current flow, but they do exhibit an energy gap caused by the Coulomb repulsion of electrons.