Air Products, Lehigh Valley, Pa., introduces its new gas-density sensor, which is designed to measure hydrogen concentration in sintering furnaces in which a nitrogen-hydrogen blend serves as the hot-zone atmosphere.
Wisconsin Oven Corp., East Troy, Mich., has manufactured a natural-gas-fired enhanced-duty walk-in oven for a transportation technology company that heat treats baskets of aluminum parts.
United States Steel Corp., Pittsburgh, announces that it will restart the second of two blast furnaces (‘A’ blast furnace) at its Granite City Works, an integrated steelmaking plant in Granite City, Ill.
Defense TechLink, Bozeman, Montana, reports that the U.S. Air Force Research Laboratory at Eglin AFB in Florida has developed USAF-96 Steel, a low-alloy steel that has demonstrated strength and toughness at −40°C even in sections up to four inches thick.