How Titanium is Made by the Kroll Process

Most titanium is now made by the Kroll process, in which titanium dioxide is reacted with chlorine to form titanium etrachloride, which is then reacted with magnesium to strip away the chlorine and leave behind the pure metal.

Thermo-Calc and QuesTek partner for advanced modeling and materials design