Kaiser Aluminum Casting Extrusion Billet
Kaiser Aluminum’s process for direct chill casting of billets A direct-chill casting system consists of a mold table on which the mold is mounted and through which water is directed to the mold, a platen-mounted bottom block, and a lined casting pit. Maximum length is determined by the depth of the casting pit. In most […]