Aerospace materials testing laboratory to expand capacity by 70%

Element Materials Technology, Huntington Beach, Calif., reports that it plans to substantially increase its aerospace testing capacity by expanding laboratory facilities by 70% and adding a third shift. The new facility will enable the laboratory to further grow its stress rupture and creep testing departments, and will house over 300 test frames, more than double its current number.

Republic Steel invests $85 million to grow production by more than one million tons

Republic Steel, Canton, Ohio, has invested $85 million at its plant in Lorain, Ohio, where it has initiated hot commissioning of its new electric arc furnace. The furnace will provide more than one million tons of steel annually for the production of semi-finished, bar, and coil products. The initial heats will be cast into 6 x 6 in. billets and will be rolled on the 0.9 in. rolling mill.

The largest jet engine gets bigger

The GE90 is already the largest and most powerful jet engine ever built. But that does not mean that GE engineers have stopped trying to make it bigger, better, and leaner.
Its new version, called GE9X, will power Boeing’s next-generation 777X aircraft. GE plans to take new high-strength carbon fiber composite blades developed for the GE9X for a spin at Boeing’s testing rig in Seattle.