Advanced Materials & Processes, Volume 173, Issue 10, November/December 2015 (ASM International)November/December 2015 Issue of Advanced Materials & Processes, featuring: Benefits of Automated Mechanical Testing; 5 Ways Materials Testing is Changing the World; Bullet-Resistant Transparent Polycrystalline Materials; iTSSe and HTPro.
One Minute Mentor: Gas Nitriding and NitrocarburizingGas nitriding is based on the decomposition of ammonia (NH3) at temperatures between 500 and 600°C (930 and 1110°F) according to: