GT Crystal Systems Furnace Produces Sapphire Boules for Cell Phone Covers GT Advanced Technologies produces large-area sapphire (aluminum oxide ceramic) substrates for scratch-free cell phone covers and high-brightness LEDs. The single-crystal sapphire is produced in furnaces that provide a highly automated operating environment capable of producing consistently uniform sapphire boules that can be cut into […]
Imaging innovation could detect acoustically invisible cracks