Spray Tips: Vibratory powder-feed devices

In addition to the powder-feeder devices most commonly used in the thermal spray industry, gravity-based devices, rotating wheel devices, and fluidized-bed systems, other systems such as vibratory powder feed devices are currently in limited use or have been used in the past.

Scientists simulate magnetization reversal of Nd-Fe-B magnets using large-scale finite element models

NIMS simulated magnetization reversal in Nd-Fe-B magnets using large-scale finite element models based on electron microscopy data. These simulations revealed microstructural features affecting coercivity, guiding the development of high-performance permanent magnets Green power generation, electric transportation, and other high-tech industries rely heavily on high-performance permanent magnets, among which the Nd-Fe-B magnets are the strongest and […]