Cummins receives federal grants to advance solid oxide fuel cells

Cummins Inc., Columbus, Ind., received two federal grants totaling $4.6 million to advance commercialization of solid oxide fuel cell (SOFC) technology, which could play a critical role in helping commercial and industrial customers reduce their carbon impact while providing energy resiliency and cutting costs.