What makes Redox flow batteries safer than lithium-ion options?
Discover how Harvard University’s innovative Redox flow battery technology offers a safer alternative to traditional lithium-ion options, especially for storing renewable energy.
3D-Micromac introduces next-generation laser sample preparation platform for whole semiconductor wafer and system-level failure analysis
High-precision analysis of 2D materials microstructures achieved using electron microscopy and machine learning
A research team led by National Institute for Materials Science, Japan, has, for the first time, produced nanoscale images of two key features in an ultra-thin material: twist domains (areas where one atomic layer is slightly rotated relative to another) and polarities (differences in atomic orientation) by combining scanning transmission electron microscopy with artificial intelligence.