Brewer Science Inc., Rolla, Mo., and Arkema France Corp. announce achievement of pilot-scale production of high-quality directed self-assembly materials using Arkema’s block copolymer technology and Brewer Science’s manufacturing expertise.
SunEdison Semiconductor initiates agreements to assure polysilicon supply
Brewer Science and Arkema produce semiconductor materials via directed self assembly
Brewer Science Inc., Rolla, Mo., and Arkema France Corp. announce achievement of pilot-scale production of high-quality directed self-assembly materials using Arkema’s block copolymer technology and Brewer Science’s manufacturing expertise.