One Minute Mentor: Make bearings more fatigue-resistant

Two ways to make bearings more fatigue-resistant in the presence of contaminated lubricants are to increase surface hardness of the rolling contact surface to minimize damage by contamination; and to make the rolling contact surfaces more damage tolerant so that surface distress caused by contaminants is less likely to initiate and propagate fatigue cracks.

New Member Survey

Welcome to ASM International. Our goal is to ensure our services and programs exceed your expectations now and in the future. In an effort to better help us understand your needs and how we can best serve you, we would appreciate your participation in our New Member Welcome Survey. {“@attributes”:{“owner-id”:”0″,”owner-type”:”3″,”default-user”:”false”,”plid”:”38686721″,”portlet-id”:”1_WAR_asmwebformportlet_INSTANCE_DcwkRd5HTIdx”},”preference”:[{“name”:”fieldReadUserFieldName7″,”value”:{}},{“name”:”fieldReadUserFieldName6″,”value”:{}},{“name”:”fieldReadUserFieldName9″,”value”:{}},{“name”:”fieldReadUserFieldName8″,”value”:{}},{“name”:”fieldReadUserExpandoFieldNames9_en_US”,”value”:”NULL_VALUE”},{“name”:”fieldReadUserFieldName3″,”value”:{}},{“name”:”fieldReadUserFieldName2″,”value”:{}},{“name”:”fieldReadUserFieldName5″,”value”:{}},{“name”:”fieldReadUserFieldName4″,”value”:{}},{“name”:”fieldReadUserFieldNames6_en_US”,”value”:”NULL_VALUE”},{“name”:”fieldReadUserFieldName1″,”value”:{}},{“name”:”databaseTableName”,”value”:”1_WAR_asmwebformportlet_INSTANCE_DcwkRd5HTIdx_7113″},{“name”:”fieldSizes10_en_US”,”value”:”NULL_VALUE”},{“name”:”fieldSizes6_en_US”,”value”:”NULL_VALUE”},{“name”:”fieldOptions9_en_US”,”value”:{}},{“name”:”fieldReadUserFieldNames12_en_US”,”value”:”NULL_VALUE”},{“name”:”fieldName10″,”value”:{}},{“name”:”fieldName11″,”value”:{}},{“name”:”fieldName12″,”value”:{}},{“name”:”fieldOptions12_en_US”,”value”:{}},{“name”:”fieldOptions4_en_US”,”value”:”Select One, 1.tOnline,2.tMail,3.tPhone,4.tOther u2013 Please Specify,”},{“name”:”fieldReadUserFieldNames1_en_US”,”value”:”NULL_VALUE”},{“name”:”emailAddress”,”value”:”[email protected]”},{“name”:”fieldOptions12″,”value”:”Article […]