ALD process developed for low-fluorine tungsten films

Lam Research Corp., Fremont, Calif., an advanced manufacturer of semiconductor equipment,introduces an atomic layer deposition process for depositing low-fluorine-content tungsten films, the latest addition to its Altus family of products.

How They Mine Copper in British Columbia

The Copper Mountain Mine is located 20 km south of Princeton, British Columbia. The 2016 production target is 80 million pounds of copper (+/– 5%), plus gold and silver byproducts. This video shows the mining process, and all the trucks and equipment needed to dig out the ore and turn it into copper.

Fluorescent microcapsules identify microscopic failure

The Autonomous Materials Systems Group at the Beckman Institute for Advanced Science and Technology, Urbana, Ill., recently devised a way to identify microscopic damage in polymers and composites by incorporating microcapsules containing materials that fluoresce under stress.