Northwest Mettech, Vancouver, announces that its NanoFeed line of liquid and suspension feeders for the thermal spray industry has been developed to enable delivery of submicron powders to thermal spray torches.
SSPC, AWS, NACE announce Public Review Period for revised thermal spray standard
The Society for Protective Coatings, the American Welding Society, and NACE International announce a public review period for its proposed Joint Standard/Standard Practice, “Specification for the Application of Thermal Spray Coatings (Metallizing) of Aluminum, Zinc, and Their Alloys and Composites for the Corrosion Protection of Steel.”