Wisconsin oven ships pin conveyor oven to automotive manufacturer

Wisconsin Oven Corp., East Troy, has shipped one electrically heated conveyor oven to an automotive manufacturer, which will be used for tempering automotive parts. The conveyor oven features a chain style conveyor system with vertical pins, ensuring the uniform transfer of parts through the heating and cooldown zones of the oven. The maximum temperature rating […]

Leading die manufacturer adds Seco/Vacuum furnace to increase capacity

Seco/Vacuum, Meadville, Pa., has announced that a U.S.-based international manufacturer has placed an order for a Vector high-pressure gas quench furnace. The new furnace will increase the partner’s heat treat capability while improving part quality. The Vector will allow the partner to heat treat larger parts, at higher quantities per cycle than their existing furnace, […]