Composite Recycling

  Video description Researchers at Oak Ridge National Laboratory (ORNL) developed a new technique to break down composite materials in order to be reused, saving time, money, and material. This research was funded by the Advanced Manufacturing Office and the Wind Energy Technologies Office at the U.S. Department of Energy. Courtesy of ORNL.