Avure HIP presses equipped with quenching furnaces improve mechanical properties

Avure Technologies, Franklin, Tenn., introduces hot isostatic presses equipped with new HIP quenching furnaces.  Variable cooling and heating rates and pressure levels make it possible to precisely control the quality and mechanical properties of treated parts. They achieve a “super-plastic” behavior, where only compressive stresses exist, voids and cracks are eliminated, and post-treatment residual stresses are very low.

New kind of microscope uses neutrons

Researchers at Massachusetts Institute of Technology, Cambridge, working with partners at NASA, developed a new concept for a microscope that would use neutrons-subatomic particles with no electrical charge-instead of beams of light or electrons to create high-resolution images.   Among other features, neutron-based instruments have the ability to probe inside metal objects-such as fuel cells, batteries, and engines, even when in use-to learn details of their internal structure.

Hubbard Receives 2013 George Bodeen Heat Treating Achievement Award

Mr. John D. Hubbard, CEO (retired), Bodycote plc, headquartered in Macclesfield, Cheshire, UK, is the recipient of the 2013 George H. Bodeen Heat Treating Achievement Award.   Established in 1996, this award recognizes distinguished and significant contributions to the field of heat treating through leadership, management, or engineering development of substantial commercial impact.

SAES Nitinol actuator elements designed for linear and rotary actuators

SAES Getters Group, Italy, offers SmartFlex Nitinol actuator elements that deliver state-of-the-art performance for reliable shape-memory-alloy actuators. Wires, springs, and components are designed for the specific requirements of any industrial actuator application. SMA wires ensure mechanical action if stimulated with electrical current, enabling the development of simple, compact, and reliable actuators.

Wooden this be some skyscraper

For HSB Stockholm’s architectural competition 2023, three teams of architects produced innovative proposals for private residences of the future at three different locations in the center of Stockholm.   Berg | C.F. Møller Architects are working in partnership with architects Dinell Johansson and consultants Tyréns on their entry. The team chose to build upwards, and has designed a 34-story residential building, which will be seen for miles.