Sciaky Inc., a subsidiary of Phillips Service Industries, Chicago, will now offer its electron beam additive manufacturing (EBAM) systems for purchase, with accelerated delivery opportunities available as early as Sept. 1.
ThyssenKrupp Steel Europe invests $121 million to modernize Duisburg continuous caster
AK Steel acquires Severstal’s Dearborn steelmaking assets
Porous silicon oxide enables high-density computer memory
Rice University, Houston, announces that its breakthrough silicon oxide technology for high-density, next-generation computer memory is one step closer to mass production, thanks to a refinement that will allow manufacturers to fabricate devices at room temperature with conventional production methods.