Reliance Steel & Aluminum Co., Los Angeles, announces that its subsidiary AMI Metals Inc., headquartered in Brentwood, Tennessee, has been awarded a multi-year contract by Lockheed Martin to provide aluminum flat-rolled plate for the F-35 Joint Strike Fighter.
3D-printed soft robotic tentacle is surprisingly agile
Unmanned Aircraft Flight Test Center
Shimadzu high-speed video camera allows ten million frames per second
Shimadzu Scientific Instruments, Japan, announces the release of its new Hyper Vision HPV-X2 high-speed video camera that features ultra-high-speed recording at ten million frames-per-second.