3D printed spine mimics bone

Stryker’s Spine division, Allendale, N.J., introduces the Tritanium Posterior Lumbar Cage, a 3D-printed intervertebral body fusion device made of Tritanium, a highly porous titanium alloy designed for bone in-growth and biological fixation.