Cornell University, Ithaca, N.Y., the University of Notre Dame, South Bend, Ind., and the semiconductor company IQE, Cardiff, Wales, put together an engineering team that has created gallium nitride (GaN) power diodes capable of serving as building blocks for future GaN power switches.