ASM International, Materials Park, Ohio, recently released ASM Handbooks Online, which features the addition of ASM Handbook, Volume 5B: Protective Organic Coatings.
Using complementary microscopy and spectroscopy techniques, researchers at say they have solved the structure of lithium- and manganese-rich transition metal oxides.
Engineers at The Ohio State University developed a new welding technique that consumes 80% less energy than a common welding technique, yet creates bonds that are 50% stronger—creating a huge impact on the auto industry.
SSAB, Sweden, announces that during the next 12 months it will release two hot-rolled advanced high-strength steel grades that exceed 800 and 1000 MPa in tensile strength for automobile chassis applications.
Seco Warwick, Meadville, Pa., introduces UniCase Master, a single flow, precision case-hardening system said to reduce distortion in gears; and the ZeroFlow gas nitriding process.