The University of Southampton, England, announces that a research group has developed a rapid deposition technology in which pulsed beams of electrons break up a gallium-lanthanum-sulfur (GLS) glass target material and deposit it as a thin film onto a substrate at a rate greater than 0.2 microns/minute.