Confluent Medical Technologies, Fremont, Calif., a leading contract manufacturer of Nitinol-based medical devices, is partnering with the Colorado School of Mines and the Alliance for the Development of Additive Processing Technologies (ADAPT) program to advance additive manufacturing methods for Nitinol.
Confluent Medical partners with consortium to develop additive manufacturing of Nitinol
Confluent Medical Technologies, Fremont, Calif., a leading contract manufacturer of Nitinol-based medical devices, is partnering with the Colorado School of Mines and the Alliance for the Development of Additive Processing Technologies (ADAPT) program to advance additive manufacturing methods for Nitinol.