Researchers at University West in Trollhättan, Sweden, have invented a friction-stir-welding tool that also functions as a temperature sensor.
Hydro may build pilot plant to test more-efficient aluminum electrolysis technology
ASB’s modernized Mesta grinder enables more accurate two-axis grinding
Ceramic screws are corrosion and heat resistant
EFD Induction article wins award
A technical paper co-authored by two senior EFD Induction R&D engineers has won a prestigious International Tube Association (ITA) award at the recently concluded Tube Düsseldorf event.