One Minute Mentor: Case Hardening
Powder metallurgy parts are case hardened to obtain higher hardness, wear, fatigue, and impact properties. The primary purpose of case hardening low-carbon steels is to provide a hard, wear-resistant surface while maintaining a soft ductile core. This combination imparts optimum wear resistance and toughness properties to these material
Gasbarre Thermal Processing Systems ships batch sintering furnace
Harper receives order for pitch carbon fiber oxidation oven system
SECO/WARWICK to deliver innovative AFT process line to Aalberts Surface Technologies
Seco/Warwick, Poland, will deliver an innovative AFT process line to Aalberts Surface. The delivery to the Dzierżoniów hardening plant includes a third main furnace, tempering furnace, and an endothermic atmosphere generator as well as loading and unloading devices along with the auxiliary infrastructure.