Ultrasonic technique reveals the identity of graphite

Scientists from Osaka University (Japan), in cooperation with neighboring Kaneka Corp., evaluated the interplanar bond strength of graphene by measuring the elastic constant of graphite, demonstrating that the elastic constant of monocrystalline graphite (top figure) was above 45 gigapascal (GPa), which was higher than conventionally believed.