Buehler, Lake Bluff, Ill., has upgraded its support of advanced manufacturing research at the Commonwealth Center for Advanced Manufacturing (CCAM) in Prince George County, Virginia.
Materials scientists at the UCLA Samueli School of Engineering and colleagues in China announce that they have developed a hydrogel coating that prevents ice from forming until the temperature reaches 23.8 degrees below zero Fahrenheit.
Wall Colmonoy, Madison Heights, Mich., announces that it will offer a spring session of Modern Furnace Brazing School on May 12-14, at Wall Colmonoy’s Aerobraze Brazing Engineering Center in Cincinnati, Ohio.
Researchers from Trinity College Dublin reported on the results of mechanical testing of Al 6061 cold spray coatings before and after a rapid heat treatment with a novel focused IR device at the ITSC 2019 conference sponsored by the Thermal Spray Society of ASM International.
Particle Testing Authority (PTA), a division of Micromeritics Instrument Corp., Norcross, Georgia, announces that it has created a comprehensive particle characterization service for the additive manufacturing industry.