Structurally Integrated Damage Tolerant Thermal Spray Coatings

Researchers from Stony Brook University’s Center for Thermal Spray Research reported in this presentation that cermet coatings applied via high-velocity thermal spray are used in aggressive wear situations and are almost always coupled with corrosive environments.