Picosun Group, Finland, reports excellent results with its next generation R&D PEALD (plasma-enhanced ALD) technology, which enables deposition at low temperatures and of several materials that could not be deposited with thermal processes only.
SEMI World Fab Forecast predicts new fab projects will reach nearly $50 billion in 2020
Cerebras Systems develops wafer scale engine chip with 1.2 trillion transistors
Seco Vacuum dual-chamber hybrid furnace provides low pressure carburizing/hardening
Lindberg three-chamber furnace integrated with robot transfer and hydraulic press
Lindberg MPH, Riverside, Mich., has built an integrated, stacked, three-chamber furnace that offers a significantly smaller footprint than a continuous system.