Ametek Edax Inc., Mahwah, N.J., introduces the OIM Matrix software package, which brings dynamic diffraction-based electron backscatter diffraction (EBSD) pattern simulations and dictionary indexing capabilities to the EBSD market.
Rigaku Corp., Japan, introduces the Nano3DX, a true X-ray microscope with the ability to deliver 3D computed tomography images of relatively large samples at high resolution.
Cree Inc., Durham, N.C., announces plans for a $1 billion investment to its headquarters in Durham to expand the company’s silicon carbide materials capabilities and wafer fabrication capacity.
Thermo Scientific, Hillsboro, Oregon, announces that with the new Thermo Scientific Meridian S inverted static Optical Fault Isolation (OFI) solution, semiconductor failure analysis labs can future-proof their operations with a fully scalable solution.
Semi, San Francisco, projects that global sales of semiconductor manufacturing equipment by original equipment manufacturers will drop by 18.4 percent to $52.7 billion in 2019 from last year’s historic high of $64.5 billion in its Mid-Year Total Equipment Forecast.