Lindberg MPH, Riverside, Mich., reports that, in the beginning of 2017, the company purchased an Ermak press brake and hydraulic swing beam shear to maximize production capabilities.
Wisconsin Oven Corp., East Troy, Wis., has built an indirect gas-fired aluminum aging oven for treating aluminum exterior components of aircraft engines.
Have you ever feared that your plane would fall apart mid-flight? Well, have no fear! Through this video, learn from engineering team leaders and aircraft assembly supervisors at Boeing why planes are so sturdy.
Aleris, Cleveland, has signed a new multi-year contract with Embraer to supply aluminum flat-rolled products for use in the production of all Embraer aircraft.