Solar Atmospheres of Western PA, Hermitage, has completed construction of a new brazing and assembly room.
EFD Sinac stationary induction heating system enables preheating in less than a second
Nitrex Metal supplies nitriding pit furnace to Voestalpine for hardening stainless steel
Nitrex Metal Inc., Quebec, announces that the High Performance Metals Division of Voestalpine AG in the Czech Republic has expanded its heat treatment capabilities with the addition of a Nitrex system for nitriding and surface hardening stainless steel for various applications.