GE Additive Arcam, Frankfurt, Germany, announces that development material (D-material) support for pure copper and highly alloyed tool steel powders will be available beginning in 2020.
Engineers from Exponent, Menlo Park, Calif., explained in a presentation at MS&T 2019 that although stainless steel is resistant to general corrosion, the failure analysis of a stainless steel hot water heater shows that it is susceptible to other modes of corrosion.
Researchers from Oxford Instruments and Manchester University reported at MS&T 2019 in Portland that rapid analyses of cracks via EBSD and EDS enable a comprehensive understanding of the dynamics of crack formation and subsequent propagation.
George Vander Voort of Vander Voort Consulting, presented a discussion of a tower design that ignored dynamic stresses, leading to the collapse of a radio tower.
Several specialty carburizing steel grades have been developed for specific requirements involving high-temperature performance, fracture toughness, and/or resistance to oxidation and corrosion.