Why plane tires don’t explode on landing

This video from Tech Insider tells about the materials in airplane tires, specifically Goodyear tires, and shows how they are made to withstand the tremendous forces of a jet landing.

ASM Media Kit

  VIEW THE ASM MEDIA KIT VIEW THE EDITORIAL CALENDAR

Contributor Corner: Erik Mueller, Ph.D.

Dr. Erik Mueller is a materials research engineer at the National Transportation Safety Board (NTSB) in Washington, DC. He has performed over 100 failure investigations of aircraft, rail, pipeline, and marine transportation accidents, including those involving the GEnx engine fan midshaft, the Boeing 787 lithium-ion battery fires, the Casselton and Heimdal, ND train derailments, and the Centreville, VA pipeline leak.