Concentrations of rare earth elements >300 ppm found in American coal basins

The U.S. Department of Energy’s National Energy Technology Laboratory, Pittsburgh, reports that its engineers have found high rare earth element concentrations in coal samples taken from the Illinois, Northern Appalachian, Central Appalachian, Rocky Mountain Coal Basins, and the Pennsylvania Anthracite region.