Cast irons typically possess higher carbon levels than steels, so that cast irons can take advantage of eutectic solidification in the binary iron-carbon system, as shown in the diagram.
Seco Vacuum supplies second vacuum heat treating furnace to global manufacturer
Constellium Alplan specialty rolled aluminum plate features up to 15 times better flatness
Constellium N.V., The Netherlands, introduces its new Alplan Beyond Precision aluminum product line, which consists of specialty rolled plates with up to 15 times better flatness compared to industry standards, up to 40 percent less material needs, and up to 90 percent reduction in part rework compared to a mill finish plate.






